GB447421A - Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys - Google Patents
Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloysInfo
- Publication number
- GB447421A GB447421A GB3315734A GB3315734A GB447421A GB 447421 A GB447421 A GB 447421A GB 3315734 A GB3315734 A GB 3315734A GB 3315734 A GB3315734 A GB 3315734A GB 447421 A GB447421 A GB 447421A
- Authority
- GB
- United Kingdom
- Prior art keywords
- aluminium
- acid
- treatment
- alloys
- relating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
447,421. Electrolytic surface treatment of aluminium and its alloys. GOWER, C. H. R., and BOWEN, E. WINDSOR-, Thames Factory, Rainville Road, Hammersmith, London. Nov. 17, 1934, No. 33157. [Class 41] The metals are coated by anodic treatment in a bath containing sulphuric acid and relatively small proportions of gallic acid and boric acid. Suitable proportions are 7-8“ fluid ounces of sulphuric acid, 0À55 ounces of gallic acid and 0À55 ounce of boric acid to 1 gallon of water. A current density of 8-12 amps. per sq. ft. and temperature 78-96‹ F., preferably 80-90‹ F., are employed. The period of treatment may be 30-40 minutes ; this is extended when the coating is to be subsequently dyed a dark colour. The coating operation may be preceded by anodic treatment for cleaning and the formation of a thin film of oxide as described in Specification 447,420.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB3315734A GB447421A (en) | 1934-11-17 | 1934-11-17 | Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB3315734A GB447421A (en) | 1934-11-17 | 1934-11-17 | Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys |
Publications (1)
Publication Number | Publication Date |
---|---|
GB447421A true GB447421A (en) | 1936-05-18 |
Family
ID=10349273
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB3315734A Expired GB447421A (en) | 1934-11-17 | 1934-11-17 | Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys |
Country Status (1)
Country | Link |
---|---|
GB (1) | GB447421A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE749287C (en) * | 1942-12-28 | 1944-11-21 | Process for the production of protective coatings on aluminum and its alloys by means of anodic oxidation | |
US2918416A (en) * | 1958-07-07 | 1959-12-22 | Taylor Paul Hunt | Electrolytic process for hard surfacing aluminum |
US3276980A (en) * | 1963-01-29 | 1966-10-04 | Gen Motors Corp | Method of anodizing aluminum |
FR2195697A1 (en) * | 1972-08-07 | 1974-03-08 | Innova Corp | Anodising aluminium to produce thick films - using boric/hydroxy carboxylic chelate acid anions with sulphuric acid |
-
1934
- 1934-11-17 GB GB3315734A patent/GB447421A/en not_active Expired
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE749287C (en) * | 1942-12-28 | 1944-11-21 | Process for the production of protective coatings on aluminum and its alloys by means of anodic oxidation | |
US2918416A (en) * | 1958-07-07 | 1959-12-22 | Taylor Paul Hunt | Electrolytic process for hard surfacing aluminum |
US3276980A (en) * | 1963-01-29 | 1966-10-04 | Gen Motors Corp | Method of anodizing aluminum |
FR2195697A1 (en) * | 1972-08-07 | 1974-03-08 | Innova Corp | Anodising aluminium to produce thick films - using boric/hydroxy carboxylic chelate acid anions with sulphuric acid |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB404251A (en) | Method of producing firmly adherent galvanic deposits on aluminium and its alloys | |
GB495190A (en) | An improved electrolytic method of coating surfaces of iron or steel | |
GB442902A (en) | Process for producing porous oxide layers on aluminium and aluminium alloys for photographic purposes | |
GB449162A (en) | Improvements in and relating to the surface treatment of aluminium and aluminium alloys | |
CN109208055B (en) | Aluminum alloy, preparation method thereof and mobile phone shell | |
CN106757235A (en) | Titanium plating treatment method for aluminum alloy surface | |
GB447421A (en) | Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys | |
GB390110A (en) | Improvements in or relating to the production of corrosion-resisting coatings on aluminium or aluminium alloys | |
GB534471A (en) | Improvements in or relating to the production of protective coatings on magnesium and magnesium alloys | |
GB447420A (en) | Improvements in and relating to the production of anodic coatings on aluminium or aluminium alloys | |
GB440608A (en) | Process for producing galvanic coatings on aluminium and its alloys | |
GB472996A (en) | Improvements in or relating to the electrodeposition of zinc | |
GB438816A (en) | Improvements relating to a protective treatment of metals and alloys | |
GB395390A (en) | Improvements in and relating to the electrolytic treatment of aluminium or its alloys | |
AU609320B2 (en) | Colour anodizing of aluminium surfaces with p-toluenesulfonic acid | |
GB469571A (en) | Process for the anodic coating of aluminium and aluminium alloys and electrolytes therefor | |
GB359495A (en) | Improvements in and relating to the production of coloured aluminium, aluminium alloys and aluminium coated articles | |
GB414966A (en) | Anodic coating of zinc base metals | |
US4100041A (en) | Method of forming a colored and oxide film on aluminum and aluminum alloys | |
GB421696A (en) | Anodic coating of zinc base metals | |
GB558726A (en) | Improvements in or relating to method of polishing copper, and electrolyte suitable for use in said method | |
GB451904A (en) | Method of electro-plating aluminium with metal | |
SU802409A1 (en) | Method of dyeing aluminium and its alloy articles | |
JPS6020478B2 (en) | Aluminum surface treatment method | |
GB378874A (en) | Improved method of and means for coating or plating metallic surfaces without the aid of electrical current or heat |