SU393352A1 - WEAR RESISTANT CAST IRON - Google Patents

WEAR RESISTANT CAST IRON

Info

Publication number
SU393352A1
SU393352A1 SU1719026A SU1719026A SU393352A1 SU 393352 A1 SU393352 A1 SU 393352A1 SU 1719026 A SU1719026 A SU 1719026A SU 1719026 A SU1719026 A SU 1719026A SU 393352 A1 SU393352 A1 SU 393352A1
Authority
SU
USSR - Soviet Union
Prior art keywords
cast iron
wear resistant
resistant cast
iron
manganese
Prior art date
Application number
SU1719026A
Other languages
Russian (ru)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1719026A priority Critical patent/SU393352A1/en
Application granted granted Critical
Publication of SU393352A1 publication Critical patent/SU393352A1/en

Description

1one

Изобретение относитс  к области изыскани  материалов, предназначенных дл  изготовлени  деталей, работающих в услови х повышенного изнапливани .The invention relates to the field of finding materials intended for the manufacture of parts operating under conditions of increased melting.

Известен чугун, содержащий хром и марганец .Known cast iron containing chromium and manganese.

Иредложенный чугун отличаетс  от известного дополнительным легированием бором и титаном. Это обеспечивает предложенному чугуну повышенную износостойкость и обрабатываемость резанием. Чугун имеет следуюш.ий состав, %: Углерод2,5-3,2The proposed cast iron is different from the known additional doping with boron and titanium. This provides the proposed cast iron increased wear resistance and machinability. Cast iron has the following composition,%: Carbon 2.5-3.2

Кремнийдо 0,8Kremniydo 0.8

Хром16-22Chrome16-22

Бор0,1-0,3Bor0,1-0,3

Титан0,2-0,4Titan0,2-0,4

Марганец0,5-1Manganese 0.5-1

Серадо 0,1Cerado 0.1

Фосфордо 0,1Fosfordo 0,1

ЖелезоОстальноеIronErest

Твердость чугуна составл ет: В литом состо нии52-56 HRCThe hardness of the iron is: In a cast state 52-56 HRC

В закаленном состо нии 58-63 HRC В отожженном состо нии 320-360 НВ Иредел прочности при изгибе 70- 100 кг/мм. Дл  повышени  износостойкости чугун закаливают от 950-980°С с охлаждением на воздухе. Обрабатываемость предложенного чугуна в 1,75-1,85 раза выше, чем аналогичного чугуна без бора и титана.In the hardened state 58-63 HRC In the annealed state 320-360 HB and bending strength 70-100 kg / mm. To increase wear resistance, the cast iron is quenched from 950-980 ° C with air cooling. The machinability of the proposed iron is 1.75-1.85 times higher than that of similar iron without boron and titanium.

Иредмет изобретени Iredmet invention

Износостойкий чугун, содержащий углерод, хром, марганец, железо, отличающийс  тем, что, с целью повышени  механических и технологических свойств, он дополнительно содержит бор и титан при следующем соотношении компонентов, %:Wear-resistant iron containing carbon, chromium, manganese, iron, characterized in that, in order to improve mechanical and technological properties, it additionally contains boron and titanium in the following ratio of components,%:

Углерод2,5-3,2Carbon2.5-3.2

Хром16-22Chrome16-22

Бор0,1-0,3Bor0,1-0,3

Титан0,2-0,4Titan0,2-0,4

Марганец0,5-1Manganese 0.5-1

ЖелезоОстальноеIronErest

SU1719026A 1971-11-25 1971-11-25 WEAR RESISTANT CAST IRON SU393352A1 (en)